Resistance Brazing
-
Published:1993
Abstract
This article presents an overview of resistance brazing (RB) used for many applications involving small workpieces, for small joints that are part of very large equipment, or for low-volume production runs. It lists the advantages and limitations of RB and outlines the factors that contribute to high quality in an RB joint. The article discusses the classification of RB such as manual RB or automatic RB. It describes the selection of metal electrodes and filler metals for RB. The filler metals include silver alloys, aluminum-silicon alloys, and copper-phosphorus alloys.
Allen Cedilote, Resistance Brazing, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 339–342, https://doi.org/10.31399/asm.hb.v06.a0001389
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.