Dip Brazing
-
Published:1993
Abstract
This article describes the dip brazing process and the principal types of furnaces used for molten-salt-bath dip-brazing applications. It provides information on equipment maintenance, which is divided into temperature control, control of the liquid, and maintenance of the vessel. The article presents the typical salts used for molten-salt dip brazing of carbon and low-alloy steels with selected filler metals in tabular form. It concludes with information on dip brazing of stainless steels, cast irons, and aluminum alloys and safety precautions of the process.
Daryl D. Peter, Dip Brazing, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 336–338, https://doi.org/10.31399/asm.hb.v06.a0001388