Selection of Wrought Precipitation-Hardening Stainless Steels
-
Published:1993
Abstract
This article commences with a brief description of the solidification characteristics and microstructures of martensitic precipitation hardening (PH) stainless steels. It reviews the welding parameters for types 17-4PH, 15-5PH, PH13-8 Mo, Custom 450, and Custom 455. The article describes the microstructural evolution and weld parameters associated with semiaustenitic PH steels. It discusses the weldability and welding recommendations for A-286 and JBK-75 austenitic PH stainless steels. The article also presents tables that list properties and heat treatments for the PH stainless steels.
B. Pollard, Selection of Wrought Precipitation-Hardening Stainless Steels, Welding, Brazing, and Soldering, Vol 6, ASM Handbook, Edited By David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards, ASM International, 1993, p 482–494, https://doi.org/10.31399/asm.hb.v06.a0001412
Download citation file:
November 12-16 | Phoenix, Arizona
Keep up-to-date at the premier event for the microelectronics failure analysis community. Register today for ISTFA 2023!