Lamina and Laminate Nonmechanical Testing
-
Published:2001
Abstract
Characterization of nonmechanical properties is performed in the testing and certification of composite materials. This article focuses on the properties of composites that are commonly investigated. The properties include: per ply thickness; constituent content; density; coefficient of thermal expansion and coefficient of moisture expansion; glass transition temperature; thermal conductivity, diffusivity, and specific heat.
Sign in
ASM members
Member Sign InJohn Moylan, Lamina and Laminate Nonmechanical Testing, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 759–765, https://doi.org/10.31399/asm.hb.v21.a0003442