Abstract
This article provides a summary of the concepts discussed in the articles under the Section “Post-Processing and Assembly” ASM Handbook, Volume 21: Composites.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Flake C. Campbell, Introduction to Post-Processing and Assembly, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 615, https://doi.org/10.31399/asm.hb.v21.a0003423
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Introduction to Reinforcing Fibers
Composites
Introduction to Composites
Composites
Introduction to Failure Analysis
Composites
Rapid Prototyping
Composites
Design with Composites
Materials Selection and Design
Guide to Materials Selection
Engineered Materials Handbook Desk Edition
Element and Subcomponent Testing
Composites
Tensile Testing of Ceramics and Ceramic-Matrix Composites
Tensile Testing (Second Edition)
Manufacturing Processes and Their Selection
Materials Selection and Design