Composites
Abstract
Braided structures are unique in their high level of conformability, torsional stability, and damage resistance. This article describes the classifications of braiding such as two-dimensional braiding and three-dimensional braiding. It presents the governing equations for computer-controlled braiding in a table. The article lists the applications of braided fabrics and composites. It discusses the formation, structure, and properties of two-dimensional braid composites and three-dimensional braid composites: the damage tolerance and the impact damage limitation.
Sign in
ASM members
Member Sign InFrank K. Ko, Braiding, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 69–77, https://doi.org/10.31399/asm.hb.v21.a0003361