Quality Assurance of Metal-Matrix Composites
By
William C. Harrigan, Jr.
William C. Harrigan, Jr.
MMC Engineering, Inc.
Search for other works by this author on:
-
Published:2001
Publication history
November 01, 2001
Abstract
This article describes the characterization techniques, mechanical tests, and nondestructive evaluation methods that are commonly used for metal-matrix composites. It also tabulates typical methods of particle size and size distribution measurement, as well as mechanical test specifications for aluminum-matrix composites.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
William C. Harrigan, Jr., Quality Assurance of Metal-Matrix Composites, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 726–730, https://doi.org/10.31399/asm.hb.v21.a0003437
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Metal-Matrix Composites
Elements of Metallurgy and Engineering Alloys
Metal-Matrix Composites
Metals Handbook Desk Edition (2nd Edition)
Metal-Matrix Composites
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Age Forming
Metalworking: Sheet Forming
Quality Control and Quality Assurance
Steel Castings Handbook (Sixth Edition)
Corrosion of Aluminum Metal-Matrix Composites
Corrosion of Aluminum and Aluminum Alloys
Sampling
Materials Characterization
Modeling and Simulation of the Heat Treatment of Aluminum Alloys
Heat Treating of Nonferrous Alloys
Process Control, Monitoring and Quality Assurance Specifics for Induction Heating
Induction Heating and Heat Treatment