Composites
Phenolic Resins
-
Published:2001
Abstract
This article describes the chemistry of phenolic resins and reviews their characteristics and properties for various composites fabrication processes. The fabrication processes include solution/hot-melt process, pultrusion, vacuum infusion, filament winding, sheet molding, and hand lay-up. The article illustrates the manufacturing process of phenolic honeycomb and provides information on the applications of phenolic composites.
Sign in
ASM members
Member Sign InShahid P. Qureshi, Phenolic Resins, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 120–125, https://doi.org/10.31399/asm.hb.v21.a0003366