Open Molding: Hand Lay-Up and Spray-Up
-
Published:2001
Abstract
Open molding is the method used in the polymer-matrix composites industry to make thermoset composite products. This article discusses the advantages, disadvantages, and applications of the open molding. It describes the various process of the open molding, such as hand lay-up process and spray-up process. Workmanship for hand lay-up and spray-up processes is reviewed. The article provides information on the matrix-resin materials used for open molding, including unsaturated polyester resins, epoxy vinyl ester resins, and reinforcements. It explains the component design and short- and long-term properties of a fiber reinforced composite laminate depending on material selection and workmanship. The...
Sign in
ASM members
Member Sign InFinn Roger Andresen, Open Molding: Hand Lay-Up and Spray-Up, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 450–456, https://doi.org/10.31399/asm.hb.v21.a0003406
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!