Design Allowables
By
Chris Boshers
Chris Boshers
Composite Materials Characterization, Inc.
Search for other works by this author on:
-
Published:2001
Publication history
November 01, 2001
Abstract
This article discusses the need for design allowables, development of design allowables, and important factors that affect the selection of the allowable. It provides a comparison between lamina and laminate allowables. The article discusses laminate results and specific techniques used in the statistical development of allowable values.
Topics
Materials design
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Chris Boshers, Design Allowables, Composites, Vol 21, ASM Handbook, Edited By Daniel B. Miracle, Steven L. Donaldson, ASM International, 2001, p 360–365, https://doi.org/10.31399/asm.hb.v21.a0003393
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Design Allowables for Static Metallic Material Properties
Mechanical Testing and Evaluation
Lamina and Laminate Mechanical Testing
Composites
Repair
Structural Composite Materials
Glossary of Filament-Winding Terms
Composite Filament Winding
Out-of-Plane Analysis
Composites
Specifications and Designations of Fibers and Resins
Composite Filament Winding
Overview of Testing and Certification
Composites
Fractography of Composites
Characterization and Failure Analysis of Plastics
Custom Sailing Yacht Design and Manufacture
Composites