Materials Selection and Design
Value Analysis in Materials Selection and Design
-
Published:1997
Abstract
Value analysis (VA) is a team problem-solving process to improve the value of a product from the viewpoint of a user. This article presents a comparison between VA and total quality management in materials selection and design. It discusses the key attributes, concepts, and activities of the VA. The application of value engineering in U.S. government contracts and the construction industry is reviewed. The article describes the eight phases of the VA process: preparation, information, analysis, creation, synthesis, development, presentation and report, and implementation and follow-up. It presents case studies that illustrate the materials-related aspects of the VA process.
Theodore C. Fowler, Value Analysis in Materials Selection and Design, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 315–321, https://doi.org/10.31399/asm.hb.v20.a0002457
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.