This article examines material property data and the information needs at various points in the design, manufacture, and use cycle. It contains a table that lists the various sources of materials data. The article describes locating media for sources of data such as suppliers of databases and internet. It discusses the types of sources of data, including computer readable media, data centers, and print media. The article also reviews the methods for evaluation and interpretation of data and examines the processes of obtaining and reporting test data.
Jack H. Westbrook, Sources of Materials Property Data and Information, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 491–506, https://doi.org/10.31399/asm.hb.v20.a0002467
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.