Design for Joining
-
Published:1997
Abstract
This article explains how to design a joint or conduct a joining process so that components can be produced most efficiently and without defects. The joining processes include mechanical fastening, adhesive bonding, welding, brazing, and soldering. The article discusses the selection and application of good design practices based on the understanding of process-related manufacturing aspects such as accessibility, quality, productivity, and overall manufacturing cost. It provides several examples of selected parts and joining processes to illustrate the advantages of a specific design practice in improving manufacturability.
K. Sampath, Design for Joining, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 762–773, https://doi.org/10.31399/asm.hb.v20.a0002488
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.