Phase Equilibria and Phase Diagram Modeling
-
Published:2009
Abstract
A phase diagram is a graphical representation of the phase equilibria of materials in terms of temperature, composition, and pressure. This article provides an overview on the background of phase diagram calculation software. It presents an algorithm to calculate binary stable phase equilibria. The article summarizes a rapid method to obtain a thermodynamic description of a multicomponent system. It also provides information on thermodynamically calculated phase diagrams.
Y.A. Chang, H.-B. Cao, S.-L. Chen, F. Zhang, Y. Yang, W. Cao, K. Wu, Phase Equilibria and Phase Diagram Modeling, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 443–457, https://doi.org/10.31399/asm.hb.v22a.a0005402
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!