Fundamentals of Modeling for Metals Processing
Internal-State Variable Modeling of Plastic Flow
-
Published:2009
Abstract
This article focuses on the analyzing and modeling of stress-strain behavior of polycrystals of pure face-centered cubic (fcc) metals in the range of temperatures and strain rates where diffusion is not important. It presents a phenomenological description of stress-strain behavior and provides information on the physical background, alternative interpretations, and directions of research. The quantitative description of strain hardening of fcc polycrystals is provided. The article also discusses the modeling of stress-strain behavior in body-centered cubic metals, hexagonal metals, stage IV work hardening, and the various classes of single-phase alloys.
Sign in
ASM members
Member Sign InH. Mecking, A. Beaudoin, Internal-State Variable Modeling of Plastic Flow, Fundamentals of Modeling for Metals Processing, Vol 22A, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2009, p 458–471, https://doi.org/10.31399/asm.hb.v22a.a0005413
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field