Materials for Medical Devices
Surface Characterization for Medical Devices
-
Published:2012
Abstract
This article focuses on the modes of operation, physical basis, sample requirements, properties characterized, advantages, and limitations of the characterization methods used to evaluate the physical morphology and chemical properties of component surfaces for medical devices. These methods include light microscopy, scanning electron microscopy, atomic force microscopy, energy-dispersive X-ray spectroscopy, Auger electron spectroscopy, secondary ion mass spectrometry, X-ray photoelectron spectroscopy, Fourier transform infrared spectroscopy, and Raman spectroscopy.
Larry D. Hanke, Surface Characterization for Medical Devices, Materials for Medical Devices, Vol 23, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2012, p 331–342, https://doi.org/10.31399/asm.hb.v23.a0005685
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.