This article discusses the composition of the major components of dental composite resins: organic resin matrix, filler, coupling agents, and initiator-accelerator systems. It describes the properties of composite resins that are related to the amount and type of filler and resin-matrix compositions. The article also discusses the compositions, properties, and clinical applications of polyacid-modified composite resins and resin-modified glass-ionomer cements. It concludes with information on biodegradation and biocompatibility of resin-based restorative materials.
Yoav Finer, Dental Composite Resins, Materials for Medical Devices, Vol 23, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2012, p 296–306, https://doi.org/10.31399/asm.hb.v23.a0005681