Nondestructive Evaluation of Materials
Reliability of Flaw Detection by Nondestructive Inspection
-
Published:2018
Abstract
The success of a reliable non-destructive evaluation (NDE) application depends greatly on the expertise and thoroughness of the NDE engineering that is performed. This article discusses the general considerations of NDE in terms of NDE response and NDE system management and schedule. It describes the NDE engineering and NDE process control, along with some case studies related to the applications of NDE. The article reviews various models for predicting NDE reliability, such as ultrasonic inspection model, eddy current inspection model, and radiographic inspection model. It concludes with an example that illustrates the integration of an ultrasonic reliability model with a CAD system.
Reliability of Flaw Detection by Nondestructive Inspection, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 23–46, https://doi.org/10.31399/asm.hb.v17.a0006443
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!