Abstract
Guided wave testing (GWT) is a method of nondestructive evaluation for the inspection of pipelines. This article focuses mainly on explaining GWT as it is applied in routine established use, covered by standards, in the oil and gas industry and also introduces some of the other contexts in which its use is growing in other evolving applications. It discusses the various guided wave modes and their selection criteria. The article provides information on considerations for mode control and the sensitivity of the GWT to the defect. It also shows some examples of advanced GWT.
Sign in
ASM members
Member Sign InMichael J.S. Lowe, Guided Wave Testing, Nondestructive Evaluation of Materials, Vol 17, ASM Handbook, Edited By Aquil Ahmad, Leonard J. Bond, ASM International, 2018, p 259–265, https://doi.org/10.31399/asm.hb.v17.a0006441
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.