Cast Iron Science and Technology
Castability, Product Design, and Production of High-Alloy Iron Castings
-
Published:2017
Abstract
Castability of alloys is a measure of their ability to be cast to a given shape with a given process without the formation of cracks/tears, pores/shrinkage, and/or other significant casting defects. This article discusses the factors which affect the fluidity of an iron melt: alloy composition and initial melt condition. Besides the basic alloy properties, the effective castability of high-alloy irons can be significantly improved through casting and casting system design. The article describes the product design and processing factors of high-alloy graphitic irons and high-alloy white irons. It explains the heat treatment of high-silicon irons for high-temperature service and concludes with a discussion on machining and finishing of high-alloy iron castings.
Harry Tian, Richard B. Gundlach, Castability, Product Design, and Production of High-Alloy Iron Castings, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 708–718, https://doi.org/10.31399/asm.hb.v01a.a0006332
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.