Modification and Inoculation of Cast Iron
-
Published:2017
Abstract
This article describes the modification and inoculation of cast iron, and schematically illustrates the major effects of inoculation in gray cast irons. Inoculation could be considered as a common liquid-state treatment for all commercial cast irons (gray/compacted/ductile irons), while modification is essential to produce compacted graphite iron (intermediate level) and ductile iron. The article discusses the most important aspects of a gray cast iron inoculation treatment and the factors influencing its inoculation efficiency. It describes the modification and inoculation of ductile cast iron and compacted graphite cast iron.
Sign in
ASM members
Member Sign InIulian Riposan, Torbjorn Skaland, Modification and Inoculation of Cast Iron, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 160–176, https://doi.org/10.31399/asm.hb.v01a.a0006315
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!