Friction, Lubrication, and Wear Technology
Environmental and Application Factors in Solid Friction
-
Published:2017
Abstract
This article focuses on environmental and application factors in solid friction. It covers the tribology of contact between a soft and hard material, including mechanisms and testing. The article describes the tribology of contact between a metal and tool during metalworking processes. It also discusses the tribology of metal friction at elevated temperatures.