Tribology and Wear of Bearing Steels[1]
Revising author
Revising author
Revising author
-
Published:2017
Abstract
This article discusses the composition, properties and applications of bearing steels. It focuses on the typical wear modes that rolling-element bearings experience: contact fatigue wear, abrasive wear, adhesive wear, and corrosive wear. The article provides information on reliability factor and ABMA and ISO environmental factors.
C.H. Hager, Jr., W.M. Hannon, V.M. Bedekar, Tribology and Wear of Bearing Steels, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 442–453, https://doi.org/10.31399/asm.hb.v18.a0006393