Friction and Wear of Polymers and Polymer Composites
-
Published:2017
Abstract
Polymers and polymer composites have become attractive for tribological applications due to their specific material properties. This article begins by discussing the fundamentals of polymer friction and wear. It summarizes the main polymer materials used in tribological applications. The article explains the effects of load, sliding velocity, and temperature on the friction coefficient. It describes three types of wear modes, namely, abrasive, adhesion, and fatigue. The article discusses the frictional behavior of polymer composites and polymer coatings. It concludes by providing information on tribotesting of polymers and polymer composites.
Nikolai K. Myshkin, Alekcander V. Kovalev, Friction and Wear of Polymers and Polymer Composites, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 559–567, https://doi.org/10.31399/asm.hb.v18.a0006373
Download citation file:
November 12-16 | Phoenix, Arizona
Keep up-to-date at the premier event for the microelectronics failure analysis community. Register today for ISTFA 2023!