Forming of Bars, Tube, and Wire
-
Published:1998
Abstract
This article discusses the mechanics, surface preparation and principles of metal forming operations such as drawing, bending (draw bending, compression bending, roll bending, and stretch bending), spinning, and straightening of bars, tubes, wires, rods and structural shapes. The article also discusses the machines and tools, including dies and mandrels, and lubricants used for these metal forming operations.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Forming of Bars, Tube, and Wire, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 811–817, https://doi.org/10.31399/asm.hb.mhde2.a0003178
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Forming of Steel Tailor-Welded Blanks
Metalworking: Sheet Forming
2014, 2014A and Alclad 2014 High-Strength Alloy
Properties and Selection of Aluminum Alloys
Forming of Copper and Copper Alloys
Metalworking: Sheet Forming
Rotary Swaging of Bars and Tubes
Metalworking: Bulk Forming
Straightening of Bars, Shapes, and Long Parts
Metalworking: Sheet Forming
5056 and Alclad 5056 Rod and Wire Alloy
Properties and Selection of Aluminum Alloys
Rod and Tube Extrusion Processes
Extrusion (Second Edition)
Induction Heating of Billets, Rods, and Bars
Induction Heating and Heat Treatment
Metalworking
Beryllium Chemistry and Processing
Bending and Forming of Tubing
Metalworking: Sheet Forming