Abstract
This article provides an overview of the composition and properties of powder metallurgy (P/M) aluminum powders for pressed and sintered parts. It includes the steps involved in the processing of high-performance P/M alloys. The article describes the classes of high-performance P/M alloys, including corrosion-resistant alloys (stress-corrosion cracking), elevated-temperature alloys, and low density/high-stiffness alloys.
You do not currently have access to this chapter.
Citation
Aluminum P/M Products, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 497–498, https://doi.org/10.31399/asm.hb.mhde2.a0003129
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Powder Metallurgy Methods and Applications
Powder Metallurgy
Forming and Shaping
Elementary Materials Science
High-Strength Aluminum Powder Metallurgy Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Fabrication and Finishing of Metal Products
Metallurgy for the Non-Metallurgist (Second Edition)
Stress-Corrosion Cracking of High-Strength Steels (Yield Strengths Greater Than 1240 MPa)
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Stress-Corrosion Cracking of Nickel-Base Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Stress-Corrosion Cracking of Titanium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Mechanisms of Stress-Corrosion Cracking
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Stress-Corrosion Cracking of Carbon and Low-Alloy Steels (Yield Strengths Less Than 1241 MPa)
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Stress-Corrosion Cracking of Stainless Steels
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)