Properties of Wrought Aluminum Alloys
-
Published:1998
Abstract
This article is a comprehensive collection of property data for wrought aluminum and aluminum alloys. Data are provided for the physical properties and mechanical properties of wrought aluminum and aluminum alloys. The listing also includes values that indicate the effect of temperatures on tensile strength, yield strength, and elongation, and the mechanical properly limits for aluminum alloy die forgings, non-heat-treatable and heat-treatable aluminum alloy sheets and plates, and non-heat-treatable aluminum alloy extruded wires, rods, bars, and shapes.
Properties of Wrought Aluminum Alloys, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 460–484, https://doi.org/10.31399/asm.hb.mhde2.a0003126
Download citation file:
Join Failure Analysis Society