Fusible alloys, eutectic and noneutectic, include a group of binary, ternary, quaternary, and quinary alloys containing bismuth, lead, tin, cadmium, and indium that melt at relatively low temperatures. This article describes the composition and mechanical properties of these alloys and lists the values of their composition and melting temperatures.
You do not currently have access to this chapter.
Citation
Fusible Alloys, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 670, https://doi.org/10.31399/asm.hb.mhde2.a0003161
Download citation file:
Related Book Content
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
Compacted Graphite Iron
Metals Handbook Desk Edition (2nd Edition)
Nickel-Base Castings
Steel Castings Handbook (Sixth Edition)
Dual-Phase Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Wear-Resistant Austenitic Manganese Steels
Metals Handbook Desk Edition (2nd Edition)
Malleable Iron
Metals Handbook Desk Edition (2nd Edition)
7039 Armor Plate
Properties and Selection of Aluminum Alloys
6069 High-Strength Extrusion Alloy
Properties and Selection of Aluminum Alloys
6262 Machinable High-Strength Alloy
Properties and Selection of Aluminum Alloys