Metals Handbook Desk Edition (2nd Edition)
Low-Expansion Alloys
-
Published:1998
Abstract
Low-expansion alloys are materials with dimensions that do not change appreciably with temperature. Alloys included in this category are various binary iron-nickel alloys and several ternary alloys of iron combined with nickel-chromium, nickel-cobalt, or cobalt-chromium alloying. Low-expansion alloys are used in various applications such as rods and tapes for geodetic surveying, moving parts that require control of expansion (such as pistons for some internal-combustion engines), bimetal strip, components for electronic devices etc. This article discusses the properties, composition, and applications of iron-nickel low-expansion alloys (Invar), as well as other special alloys, including iron-nickel-chromium alloys, iron-nickel-cobalt alloys, iron-cobalt-chromium alloys, and...
Sign in
ASM members
Member Sign InLow-Expansion Alloys, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 665–667, https://doi.org/10.31399/asm.hb.mhde2.a0003159
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!