Alloy and Temper Designation Systems for Aluminum
-
Published:1998
Abstract
This article describes the systems for designating the aluminum and aluminum alloys that incorporate the product forms (wrought, casting or foundry ingots) and its respective temper for strain-hardened alloys, heat-treatable alloys and annealed alloys. All these systems are covered by American National Standards Institute (ANSI) standard H35.1. Furthermore, the article provides a short note on the designation of unregistered tempers.
Alloy and Temper Designation Systems for Aluminum, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 423–426, https://doi.org/10.31399/asm.hb.mhde2.a0003122