Precious Metals and Alloys
-
Published:1998
Abstract
Precious metals include gold, silver, and six platinum-group metals, namely, platinum, palladium, ruthenium, rhodium, osmium, and iridium. This article focuses on the consumption, trade practices, properties, product forms, and applications of these metals and their alloys.
Topics
Properties and performance,
Material failure analysis,
Fractography,
Cast iron,
Steel,
Stainless steel,
High-strength low-alloy steel,
Steel powder,
Superalloys,
Metallography,
Aluminum,
Processing, treatment, and fabrication,
Metal products,
Mechanical properties,
Physical properties,
Gold,
Silver
You do not currently have access to this chapter.
Citation
Precious Metals and Alloys, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 624–628, https://doi.org/10.31399/asm.hb.mhde2.a0003150
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Corrosion of Precious Metals and Alloys
Corrosion: Materials
Miscellaneous Nonferrous Metals
Elements of Metallurgy and Engineering Alloys
Noble and Precious Metal Applications in Biomaterials with Emphasis on Dentistry
Materials for Medical Devices
Properties of Precious Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Annealing of Precious Metals
Heat Treating of Nonferrous Alloys
History of Powder Metallurgy
Powder Metallurgy
Precious Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Stress-corrosion Fracture in Silver Solid-State Bonds of Uranium
Handbook of Case Histories in Failure Analysis
Electrostatic Discharge Attack on a Thrust Bearing Face in a Power Turbine
Handbook of Case Histories in Failure Analysis