Metals Handbook Desk Edition (2nd Edition)
Principles and Procedures of Fractography
-
Published:1998
Abstract
Fractography is the systematic study of fractures and fracture surfaces. It is a useful tool in failure analysis and provides a means for correlating the influence of microstructure on the fracture mode of a given material. This article discusses the preservation, preparation, and photography of fractured parts and surfaces, and describes some of the more common fractographic features revealed by light microscopy, including tensile-fracture surface marks in unnotched specimens, fatigue marks, and structural discontinuities within the metal. The article also explains how to interpret fracture information contained in optical and scanning-electron microscope fractographs.
Sign in
ASM members
Member Sign InPrinciples and Procedures of Fractography, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 1238–1247, https://doi.org/10.31399/asm.hb.mhde2.a0003226
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field