General Introduction to Surface Engineering
-
Published:1998
Abstract
This article is a general introduction to surface engineering of engineering components, providing an overview of the applications of surface treatments and the environmental protection regulations directly or indirectly related to surface engineering processes.
Topics
Properties and performance,
Material failure analysis,
Fractography,
Cast iron,
Steel,
Stainless steel,
High-strength low-alloy steel,
Steel powder,
Superalloys,
Metallography,
Aluminum,
Processing, treatment, and fabrication,
Mechanical and machine components,
Surface treatment,
Surface properties
You do not currently have access to this chapter.
Citation
General Introduction to Surface Engineering, Metals Handbook Desk Edition, 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 1125–1126, https://doi.org/10.31399/asm.hb.mhde2.a0003212
Download citation file:
Related Book Content
Foreword
Introduction to Thin Film Deposition Techniques: Key Topics in Materials Science and Engineering
Preface
Introduction to Thin Film Deposition Techniques: Key Topics in Materials Science and Engineering
About the Author
Introduction to Thin Film Deposition Techniques: Key Topics in Materials Science and Engineering
Engineering Component Configuration
Aluminum Castings Engineering Guide
Fatigue Fracture Appearances
Failure Analysis and Prevention (2021 Edition)
Surface Engineering of Nonferrous Metals
Metals Handbook Desk Edition (2nd Edition)
Low-Energy Ion-Scattering Spectroscopy
Materials Characterization
Electron Beam Surface Hardening
Steel Heat Treating Fundamentals and Processes
Thermal Aspects of Surface Finishing Processes
Surface Engineering
Anodizing
Surface Engineering