Design and Engineering Properties of Glasses
-
Published:1995
Abstract
This article describes the chemical composition, physical properties, thermal properties, mechanical properties, electrical properties, optical properties, magnetic properties, and chemical properties of glasses, glass-matrix composites, and glass-ceramics.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Design and Engineering Properties of Glasses, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 1171–1187, https://doi.org/10.31399/asm.hb.emde.a0003066
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
Properties of Pure Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Physical Properties of Metals
Elements of Metallurgy and Engineering Alloys
Properties of Precious Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Cast Copper Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Zinc and Zinc Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Wrought Aluminum and Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Wrought Coppers and Copper Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Effects of Composition, Processing, and Structure on Properties of Engineering Plastics
Materials Selection and Design
Crystallography and Engineering Properties of Ceramics
Engineered Materials Handbook Desk Edition
Low-Expansion Alloys
Metals Handbook Desk Edition (2nd Edition)