Engineered Materials Handbook Desk Edition
Hand Lay-Up, Spray-Up, and Mechanical Lay-Up
-
Published:1995
Abstract
Wet lay-up using hand or spray techniques is one of the simplest methods of combining a fiber reinforcement with a solidifying resin to form a composite structure. This article describes several wet lay-up processes - including contact molding, spray molding, vacuum bag molding, and autoclave molding - suited for making parts on open-faced molds using polyester and vinyl ester resins. The article also provides information on mechanically assisted lay-up which can be automated to alleviate some of the manual work.
Sign in
ASM members
Member Sign InHand Lay-Up, Spray-Up, and Mechanical Lay-Up, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 539–545, https://doi.org/10.31399/asm.hb.emde.a0003036
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field