Engineering Tables: Ceramics and Glasses
-
Published:1995
Abstract
This article is a comprehensive collection of engineering property data in tabulated form for ceramics and glasses. Data are provided for physical and mechanical properties of ceramic materials and color of ceramics fired under oxidizing and reducing conditions. The article also lists the materials characterization techniques for ceramics and glasses.
You do not currently have access to this chapter.
Citation
Engineering Tables: Ceramics and Glasses, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 103–105, https://doi.org/10.31399/asm.hb.emde.a0003004
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Characterization of Ceramics and Glasses
Materials Characterization (2019 Edition)
Introduction to Materials Characterization
Materials Characterization
Mechanical Behavior of Nonmetallic Materials
Mechanics and Mechanisms of Fracture An Introduction
Fatigue Testing of Brittle Solids
Mechanical Testing and Evaluation
Ceramic Materials
Materials for Medical Devices
Acoustic Microscopy
Nondestructive Evaluation of Materials
Glossary of Terms: Materials Characterization
Materials Characterization
Design and Engineering Properties of Glasses
Engineered Materials Handbook Desk Edition
Introduction to the Mechanical Behavior of Nonmetallic Materials
Mechanical Testing and Evaluation
Temper Colors for Steels
Heat Treating of Irons and Steels