Introduction to Polymer-Matrix Composites
-
Published:1995
Abstract
This article discusses the types, properties, and uses of continuous-fiber-reinforced composites, including glass, carbon, aramid, boron, continuous silicon carbide, and aluminum oxide fiber composites. While polyester and vinyl ester resins are the most used matrix materials for commercial applications, epoxy resins, bismaleimide resins, polyimide resins, and thermoplastic resins are used for aerospace applications. The article addresses design considerations as well as product forms and fabrication processes.
You do not currently have access to this chapter.
Citation
Introduction to Polymer-Matrix Composites, Engineered Materials Handbook Desk Edition, Edited By Michelle M. Gauthier, ASM International, 1995, p 469–475, https://doi.org/10.31399/asm.hb.emde.a0003031
Download citation file:
Related Book Content
Introduction to Constituent Materials
Composites
Ceramic-Matrix Composites
Engineered Materials Handbook Desk Edition
Failure Causes
Composites
Mechanical Testing of Polymers
Engineered Materials Handbook Desk Edition
Polymer-Matrix Composites
Lightweight Materials Understanding the Basics
Introduction to Post-Processing and Assembly
Composites
Void Analysis of Composite Materials
Optical Microscopy of Fiber-Reinforced Composites
Aluminum—The Light Metal
The History of Metals in America