Mechanical Testing and Evaluation
Mechanical Testing of Threaded Fasteners and Bolted Joints
-
Published:2000
Abstract
This article provides an overview of the relationships between torque, angle-of-turn, tension, and friction and explains how they are measured and evaluated. It focuses on the principle, test equipment, procedure, evaluation, and test report of various testing methods, namely, friction coefficient testing, torque tension testing, locknut testing, and angular ductility and rotational capacity tests. The article reviews the basic methods and fundamental principles for mechanical testing of externally and internally threaded fasteners and bolted joints. The test methods for externally threaded fasteners include product hardness, proof load, axial and wedge tension testing of full-sized products, tension testing of machined...
Sign in
ASM members
Member Sign InRalph S. Shoberg, Mechanical Testing of Threaded Fasteners and Bolted Joints, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 811–835, https://doi.org/10.31399/asm.hb.v08.a0003323
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field