Miscellaneous Hardness Tests
-
Published:2000
Abstract
Miscellaneous hardness tests encompass a number of test methods that have been developed for specific applications. These include dynamic, or "rebound," hardness tests using a Leeb tester or a Scleroscope; static indentation tests on rubber or plastic products using the durometer or IRHD testers; scratch hardness tests; and ultrasonic microindentation testing. This article reviews the procedures, equipment, and applications associated with these alternate hardness test methods.
Sign in
ASM members
Member Sign InEdward L. Tobolski, Miscellaneous Hardness Tests, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 252–259, https://doi.org/10.31399/asm.hb.v08.a0003275