Book Chapter
Microindentation Hardness Testing
By
George F. Vander Voort
George F. Vander Voort
Buehler Ltd.
Search for other works by this author on:
-
Published:2000
Abstract
This article provides a discussion on the equipment used and specimen preparation for microindentation hardness testing (MHT) such as the Vickers hardness test and the Knoop hardness test. It describes the important test considerations to be considered during MHT. The article also discusses the most common hardness conversions and the applications of MHT.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
George F. Vander Voort, Microindentation Hardness Testing, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 221–231, https://doi.org/10.31399/asm.hb.v08.a0003272
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Process Capability and Tolerances
Steel Castings Handbook (Sixth Edition)
Overview of Wear and Erosion Testing of Coatings
Surface Engineering
Selection and Industrial Applications of Hardness Tests
Mechanical Testing and Evaluation
Tensile Testing Equipment and Strain Sensors
Tensile Testing (Second Edition)
Design Criteria
Composites
Specimen Preparation for Light Microscopy
Metallography Principles and Practice
Scanning Electron Microscopy
Fractography
Optical Metallography
Materials Characterization
Mechanical Property Test Methods
Structural Composite Materials
Metallographic Specimen Preparation
Metallographer’s Guide Practices and Procedures for Irons and Steels