Immersion Testing
-
Published:2003
Abstract
Immersion testing is the most frequently conducted test for evaluating corrosion of metals in aqueous solutions. This article focuses on the basic factors that are considered in different conditions of immersion testing. These factors are solution composition, temperature, aeration, volume, velocity, and waterline effects; specimen surface preparation; method of immersion of specimens; duration of test; and method of cleaning specimens. The article discusses the different conditions of immersion testing, namely, full immersion condition, high temperature condition, partial immersion and vapor phase condition, and alternate immersion condition. It concludes with a checklist of items that should be included in a standard report of immersion tests.
Te-Lin Yau, Immersion Testing, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 463–469, https://doi.org/10.31399/asm.hb.v13a.a0003645
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!