Corrosion: Fundamentals, Testing, and Protection
Evaluating Microbiologically Influenced Corrosion
-
Published:2003
Abstract
This article explains how an engineer might go about assessing the risk of microbiologically influenced corrosion (MIC) in an industrial situation. It describes the systems that are susceptible to the effects of MIC by sulfate-reducing bacteria (SRB). The article discusses the effects of microorganisms other than SRB on metals. SRB-related problems, which are the most common MIC issue, are also explored. The article describes the test procedures used to enumerate microbiological populations. It concludes with a discussion on risk assessment based on operating conditions.
James F.D. Stott, Evaluating Microbiologically Influenced Corrosion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 644–649, https://doi.org/10.31399/asm.hb.v13a.a0003670
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.