Abstract
This article provides an introduction to the fundamentals of corrosion in gases. It tabulates the structures and properties of oxides as well as the physical properties of pure metals.
Topics
Corrosion,
Environmentally induced corrosion,
Localized corrosion,
Microbiologically-influenced corrosion,
Mechanically assisted corrosion,
Metallurgically influenced corrosion,
Corrosion inhibitors,
Corrosion testing,
Physical properties,
Ferrous metals and alloys,
Nonferrous metals and alloys
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Marek Danielewski, Introduction to Fundamentals of Corrosion in Gases, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 87–89, https://doi.org/10.31399/asm.hb.v13a.a0003716
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Effects of Metallurgical Variables on Aqueous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Thermodynamics of Gaseous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Failure of Copper Rivets Due to “Gassing”
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Atlas of Microstructures
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Electrochemical Refining
Corrosion: Fundamentals, Testing, and Protection
Solidification Structures of Pure Metals
Metallography and Microstructures
Etchants for Revealing Microstructure
Metallography Principles and Practice
Melting of Glasses and Oxides
Induction Heating and Heat Treatment
Electrical Contact Materials
Metals Handbook Desk Edition (2nd Edition)
Failure of Steam Pipe at Local Defects
ASM Failure Analysis Case Histories: Power Generating Equipment