Abstract
This article presents an overview of the science and engineering of materials along with suitable definitions, descriptions, and examples for better understanding for corrosionists with limited field knowledge. It begins with a detailed description of various categories of engineering materials and moves into the discussion of physical properties of materials, such as the phases, strength, conductivity, and wear. The article describes the methods used in the fabrication of engineering materials and summarizes the materials and their properties in a tabular form. The article concludes with information on material design, materials applications, and materials failure analysis.
Wayne Reitz, James Rawers, Materials Basics for the Corrosionist, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 980–991, https://doi.org/10.31399/asm.hb.v13a.a0003711
Download citation file:
New Handbook: Volume 11B
Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.