This article presents a detailed discussion on the relative performance properties of principal rubber types used in lining applications together with their application, vulcanization and inspection techniques, and material and installation costs.
You do not currently have access to this chapter.
Citation
E. Bud Senkowski, Kenneth B. Tator, Rubber Coatings and Linings, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 845–850, https://doi.org/10.31399/asm.hb.v13a.a0003695
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.
Related Book Content
Stud Arc Welding
Welding Fundamentals and Processes
Failure of a Large Oil Storage Tank
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Guide to Nondestructive Evaluation Techniques
Nondestructive Evaluation of Materials
High-Frequency Welding
Welding, Brazing, and Soldering
Forging of Magnesium Alloys
Metalworking: Bulk Forming
High-Frequency Welding
Welding Fundamentals and Processes
Electrochemical Techniques for In-Service Corrosion Monitoring
Corrosion: Fundamentals, Testing, and Protection
Standards and Inspection
Practical Induction Heat Treating (Second Edition)
Surface Preparation
Protective Organic Coatings
CAD/CAM Applications in Machining
Machining