Abstract
This article describes the various factors that affect the extent of corrosion resulting from galvanic coupling. The factors include galvanic series, polarization behavior, and geometric relationship of metals and alloys. The article briefly discusses the various modes of attack that lead to galvanic corrosion of anodic members. It also explains the three electrochemical techniques of screening tests for predicting galvanic corrosion. The electrochemical techniques comprise of potential measurements, current measurements, and polarization measurements. The article provides a detailed discussion on the performance of alloy groupings. It concludes with information on various control methods that reduce or eliminate galvanic-corrosion effects.
Robert Baboian, Galvanic Corrosion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 210–213, https://doi.org/10.31399/asm.hb.v13a.a0003607
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field.