Evaluating Exfoliation Corrosion
Revising author
-
Published:2003
Abstract
Exfoliation is a structure-dependent form of localized intergranular corrosion that follows grain boundaries in the rolling direction of wrought materials, particularly aluminum alloys. Highly cold-worked materials with elongated grain boundaries tend to be most affected. The article provides information on accelerated salt spray and total-immersion testing methods to help rate the exfoliation corrosion susceptibility of various aluminum alloys and alloy compositions. It also discusses visual assessment challenges and identifies several ASTM designations and where and how they apply.
Bopinder Phull, Evaluating Exfoliation Corrosion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 572–574, https://doi.org/10.31399/asm.hb.v13a.a0003665
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!