Analysis of the Effects of Lightning Strikes on Polymeric Composites[1]
-
Published:2004
Publication history
February 26, 2011
Abstract
Lightning damage in polymer composites is manifested by damage at both the macroscopic or visual level and within the material microstructure. This article illustrates the effects of the laboratory-generated lightning strikes on polymeric composites.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Brian S. Hayes, Luther M. Gammon, Analysis of the Effects of Lightning Strikes on Polymeric Composites, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, https://doi.org/10.31399/asm.hb.v09.a0009085
Download citation file:
Join Failure Analysis Society
The ASM Failure Analysis Society (FAS) is a community where failure analysis professionals from all over the world can learn and grow in their field
Related Book Content
The Effects of Lightning Strikes on Polymeric Composites
Optical Microscopy of Fiber-Reinforced Composites
Surface Degradation of Composites
Optical Microscopy of Fiber-Reinforced Composites
Wear Failures of Reinforced Polymers
Characterization and Failure Analysis of Plastics
Metallographic Techniques for Tool Steels
Metallography and Microstructures
The Failure Analysis Process
Fatigue and Fracture Understanding the Basics
Pipeline Failure Results from Lightning Strike: Act of Mother Nature?
Handbook of Case Histories in Failure Analysis
Examination of Damage and Material Evaluation
Failure Analysis and Prevention (2021 Edition)
Examination of Damage and Material Evaluation
Failure Analysis and Prevention
Friction and Wear of Polymers and Polymer Composites
Friction, Lubrication, and Wear Technology