Abstract
Polymer composite materials are subject to degradation if not appropriately protected from the environment. This article describes the effects of heat and atomic oxygen and ultraviolet-light on composite material surfaces, with illustrations.
You do not currently have access to this chapter.
Citation
Brian S. Hayes, Luther M. Gammon, Analysis of Surface Degradation of Composites, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, https://doi.org/10.31399/asm.hb.v09.a0009084
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.
Related Book Content
Surface Degradation of Composites
Optical Microscopy of Fiber-Reinforced Composites
Temper Colors for Steels
Heat Treating of Irons and Steels
Heat Treatment of Wrought Nickel Alloys
Heat Treating of Nonferrous Alloys
Effect of Environment on the Performance of Plastics
Failure Analysis and Prevention