Book Chapter
Bainitic Structures
By
Matthew J. Perricone
Matthew J. Perricone
Lehigh University
Search for other works by this author on:
-
Published:2004
Abstract
This article provides a discussion on the transformations of various categories of bainite in ferrous systems. These include upper bainite, lower bainite, inverse bainite, granular bainite, and columnar bainite. The article also provides information on the bainite transformations in nonferrous systems.
You do not currently have access to this chapter.
Citation
Matthew J. Perricone, Bainitic Structures, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 179–185, https://doi.org/10.31399/asm.hb.v09.a0003739
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Periodic Table of Elements
Fundamentals of Modeling for Metals Processing
Massive Transformation Structures
Metallography and Microstructures
Voltammetry
Materials Characterization
Mössbauer Spectroscopy
Materials Characterization
Introduction to Structures in Metals
Metallography and Microstructures
Small-Angle X-Ray and Neutron Scattering
Materials Characterization
Ion Chromatography
Materials Characterization
Introduction: Atlas of Fractographs
Fractography
Gases in Metals
Casting
Boriding (Boronizing) of Metals
Steel Heat Treating Fundamentals and Processes